Halogen content of penetrant materials is limited because of the possibility of stress corrosion cracking in which of the following materials? |
| A. | High tensile steel |
| B. | Austenitic stainless steel |
| C. | Titanium alloys |
| D. | All of the above |
| Answer» D. All of the above | |