Q.

which of the following methods are used ot reduce galvanic corrosion ?

A. select two metals that are close together in the galvanic corrosion
B. avoid relatively small area of less noble metal and large area of more noble metal
C. insulate the metal from each other
D. all of the above
Answer» D. all of the above