| Q. |
Surface analysis can provide information that classic methods like microscopic cannot. |
| A. | true |
| B. | false |
| Answer» A. true | |
| Explanation: surface analysis can provide information that classic methods like microscopic cannot. it is better than reflectivity, adsorption isotherms, etc. | |
View all MCQs in
Fundamentals of NanoScienceNo comments yet